PT Journal AU Tavodova, M Vargova, M Krilek, J Stancekova, D TI Analysis of Damaged Delimber Knives and the Possibility of Increasing their Service Life SO Manufacturing Technology Journal PY 2022 BP 80 EP 88 VL 22 IS 1 DI 10.21062/mft.2022.011 DE delimber knives; HARDOX 450; microstructure; hard facing; wear AB The article deals with the wear of the blades of the delimber device of harvester head. An input analysis of the materials of the fixed knife and movable arm parts was performed. It consisted of chemical analysis, evaluation of microstructure and hardness measurement by HRC and HB methods. The original welded joint was analyzed, which ensured the connection of the blade and the fixed, resp. movable arm mechanism. Based on the findings, two blade replacement solutions have been proposed. The first was the application of hard metal by an OK 84.58 electrode and second use HARDOX 450 by welding with a fixed part or a mechanical gripping with screws. This was recommended based on previous research at the Faculty of Technology. The hardnesses of the original blade material were compared with the proposed solutions. The correctness of the proposed methods will be verified in the future and in operation. ER