Manufacturing Technology 2024, 24(5):834-842 | DOI: 10.21062/mft.2024.079

Effects of Laser Shock Peening Technology on Stress Corrosion Cracking of Austenitic Steel

Jana Zavitkovská ORCID..., Zdeněk Fulín ORCID..., Zbyněk ©pirit ORCID...
Centrum výzkumu Řeľ s.r.o., Hlavní 130, Řeľ, 250 68 Husinec, Czech Republic

This article deals with the modification of surface properties of austenitic steels using laser shock peening (LSP) technology. This technology introduces residual compressive stresses into the surface layer. These stresses improve the technical properties of the material not only by affecting the re-sistance of corrosion cracking under stress. The aim of the work was to influence the austenitic steel 08CHN10T by LSP technology, to perform a corrosion test in a boiling MgCl2 solution and the sub-sequent evaluation of these tests. Furthermore, the hardness was measured of the peened part of the material by LSP technology and unpeened part.

Keywords: LSP, 08CH18N10T, Corrosion, Stress corrosion cracking, Residual stress
Grants and funding:

The presented results were obtained using the CICRR infrastructure financially supported by the Ministry of Education, Youth and Sports
The presented work has been realized within Institutional Support by Ministry of Industry and Trade of the Czech Republic. The experimental results were obtained in the framework of sub-objective 12 of this project

Received: December 11, 2023; Revised: October 3, 2024; Accepted: October 22, 2024; Prepublished online: November 27, 2024; Published: November 28, 2024  Show citation

ACS AIP APA ASA Harvard Chicago Chicago Notes IEEE ISO690 MLA NLM Turabian Vancouver
Zavitkovská J, Fulín Z, ©pirit Z. Effects of Laser Shock Peening Technology on Stress Corrosion Cracking of Austenitic Steel. Manufacturing Technology. 2024;24(5):834-842. doi: 10.21062/mft.2024.079.
Download citation

References

  1. Materials Reliability Program: Technical Basis for Primary Water Stress Corrosion Cracking Mitigation by Surface stress Improvement, (2016) (MRP-267, Revision 2), EPRI Project, 380
  2. DING, K., YE., L., (2006) Laser shock peening, Performance and process simulation, Woodhead Publishingon behalf of The Institute of Materials, Minerals and Mining, Cambridge England, 151-157 Go to original source...
  3. CLAURER, A.H., GREGORY, J.K., RACK, H.J., EYLON, D., (eds), Laser shock peening for fatigue resistence. Proceedings of Surface Performance of Titanium, TMS, Warrendale, PA. Metal Society of AIME, 217-230
  4. SPIRIT, Z., KAUFMAN, J., STREJCIUS, J., CHOCHOLOUSEK, M. and KOTT, J., 2019. Increase of the Fatigue Life of Stainless Steel by Laser Shock Peening. DAAAM Proceedings, pp.0826-0831 Go to original source...
  5. ©PIRIT, Z., BRAJER, J., KAUFMAN, J., CHOCHOLOU©EK, M., BOHM, M., KOTTt, J. and STREJCIUS, J., 2018. Effect of Laser Shock Peening on Fatigue life of Austenitic stainless steels. IOP Conference Series: Materials Science and Engineering Go to original source...
  6. KAUFMAN, J., ©PIRIT, Z., VASUDEVAN V., STEINER, M., MANNAVA, S., BRAJER, J., PÍNA, L. and MOCEK, T., 2021. Effect of Laser Shock Peening Parameters on Residual Stresses and Corrosion Fatigue of AA5083. Metals, 11(10), p.1635. 2 Go to original source...
  7. CHAMPAIGNE, J., (2006) History of Shot Peening Specifications, Ninth International Conference on Shot Peening, 12-13, 38
  8. FAIRAND, A.H., CLAUER, A., AIRAND, A.H.,CLAUER, B.P., (1979) Interaction of laser-induced stress waves with metals. Proceedings of the ASM Conference Applications of Lasers in Materials Processing, Washington, DC, USA, 18-20 April 1979; ASM International: Materials Park, OH, USA,
  9. FAIRAND, B.P., WILCOX, B.A., GALLAGHER, W.J.,WILLIAMS, D.N.,(1972) Laser shock-induced micro-structural and mechanical property changes in 7075 aluminum. J. Appl. Phys. Go to original source...
  10. GJUBA, A. K., MEDRAJ, M. (2014) Laser Peening Process and Its Impact on Materials Properties in Comparison with Shot Peening and Ultrasonic Impact Peening. Materials (Basel). 7926-7962 Go to original source...
  11. BRAJAR, J., (2014) Application of laser shock peening, CVUT.
  12. Materials Reliability Program: Technical Basis for Primary Water Stress Corrosion Cracking Mitigation by Surface Stress Improvement (2016)(MRP-267, Revision 2), EPRI Project 1-1 - 2-35
  13. Materials Reliability Program: Technical Basis for Primary Water Stress Corrosion Cracking Mitigation by Surface Stress Improvement (2016)(MRP-267, Revision 2), EPRI Project 1-1 - 2-35
  14. GUJBA, ABDULLAHI K., and MAMOUM M. 2014. Laser Peening Process and Its Impact on Materials Properties in Comparison with Shot Peening and Ultrasonic Impact Peening. Materials 7, no. 12: 7925-7974. https://doi.org/10.3390/ma7127925 Go to original source...
  15. BRICÍN, D., ©PIRIT, Z., GILÍK, H. & KAUFMAN, J. 2024. Effect of Laser Shock Peening on the Micro-structure of P265GH Steel and X6CrNiTi18-10 Stainless Steel Dissimilar Welds. Manufacturing Technology, 24, 9-14. Go to original source...
  16. BRAJER, J., MÁDL, J., ©VÁBEK, R., PITRMUC, Z., ROSTOHAR, D., ZEMAN, P. & OCAÑA, J.L. 2015. Application of Laser Shock Processing. Manufacturing Technology, 15, 278-85. Go to original source...
  17. PROCHAZKA, J., VILIS, J., DOBROCKY, D. & SPERKA, P. 2022. Modification of Diffusion Layers by Laser Shock Peening. Manufacturing Technology, 22, 724-32. Go to original source...

This is an open access article distributed under the terms of the Attribution-NonCommercial 4.0 International License (CC BY-NC 4.0), which permits non-comercial use, distribution, and reproduction in any medium, provided the original publication is properly cited. No use, distribution or reproduction is permitted which does not comply with these terms.